Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0093 cm/cm @Time 86400 sec |
0.0093 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0093 cm/cm @Time 86400 sec |
0.0093 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0093 cm/cm @Time 86400 sec |
0.0093 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0093 cm/cm @Time 86400 sec |
0.0093 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0093 cm/cm @Time 86400 sec |
0.0093 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |