SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Konduit
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Physical Properties Metric English Comments
Density 2.04 g/cc
0.0737 lb/in³
ASTM D792
Moisture Absorption 0.300 %
0.300 %
23°C / 50% RH; ISO 62
0.300 %
0.300 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Time 86400 sec
0.0090 in/in

@Time 24.0 hour
ASTM D955
0.0093 cm/cm

@Time 86400 sec
0.0093 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0146 cm/cm

@Time 86400 sec
0.0146 in/in

@Time 24.0 hour
ISO 294
0.015 cm/cm

@Time 86400 sec
0.015 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ISO 527
101 MPa
14600 psi
ASTM D638
Elongation at Break 1.4 %
1.4 %
ASTM D638
1.8 %
1.8 %
ISO 527
Tensile Modulus 11.92 GPa
1729 ksi
1 mm/min; ISO 527
13.1 GPa
1900 ksi
50 mm/min; ASTM D638
Flexural Strength 174 MPa
25200 psi
ISO 178
182 MPa
26400 psi
ASTM D790
Flexural Modulus 11.25 GPa
1632 ksi
ISO 178
11.44 GPa
1659 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.53 J/cm
8.49 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 J
7.38 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Thermal Conductivity 1.20 W/m-K
8.33 BTU-in/hr-ft²-°F
ASTM E 1530
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
421 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
226 °C

@Thickness 3.20 mm
439 °F

@Thickness 0.126 in
unannealed; ASTM D648