Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.011 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
DAM
Aardvark Polymers Aarlon® 4055FR PA 6/6 Rotational Molding Resin
Aarlon 4055FR is a premium flame retardant type 6/6 nylon.Aarlon 4055FR is halogen, heavy metal, and red phosphorus free.Aarlon 4055FR is UL94 V-0 rated.Aarlon 4055FR is semi-crystalline, nucleated,..
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer
LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66
LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific)
LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66
LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific)
LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12
LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific)
LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific)
LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific)
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp PH0390A PA 6
LNP THERMOCOMP* PH0390A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6
LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific)
LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
DAM
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MFD02 PP
LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Time 86400 sec
0.011 - 0.013 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific)
LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Time 86400 sec
0.011 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).