Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66
LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific)
LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66
LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific)
LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).