Polymer Property : K Factor (ISO) = 1100 µm/km Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K Factor (ISO) 1100 µm/km
1100 µm/km
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)
Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan..