Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 1100 µm/km | 1100 µm/km | |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |