Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 60 µm/km | 60 µm/km | |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
K Factor (ISO) | 60 µm/km | 60 µm/km | |
Quadrant EPP Quadrant LSG PC extruded (ISO Data) Within its portfolio of Life Science Grade Engineering Plastic Products - specifically developed for applications in the medical, pharmaceutical and biotechnology industries - Quadrant offers QUADRA.. |