Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 0.827 MPa | >= 120 psi | ASTM D3574-75 Test E |
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Tensile Strength | >= 0.827 MPa | >= 120 psi | ASTM D3573 Test E |
Rogers Corporation R/bak® SF Supported Firm Cushion Mounting Material R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b.. |
|||
Tensile Strength | >= 0.827 MPa | >= 120 psi | ASTM D3573 Test E |
Rogers Corporation R/bak® U Unsupported Cushion Mounting Material R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b.. |
|||
Tensile Strength | >= 0.827 MPa | >= 120 psi | ASTM D3573 Test E |
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b.. |
|||
Tensile Strength | >= 0.827 MPa | >= 120 psi | |
P & P Technology A320C UL Neoprene/EPDM SAE J18 Specification: 2C2 ASTM Specification: 2C2 (1985&91). SCE42 (1967&68). RE42E1 (1978)Flame Resistance: Pass UL94V-0, HBF, HF-1**, GM609OMB4,A FMVSS302 Pass @ 0.8mm.IMDS Node ID: 13900758Infor.. |
|||
Tensile Strength | >= 0.827 MPa | >= 120 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i.. |
|||
Tensile Strength | >= 0.827 MPa | >= 120 psi | ASTM D412 |
Parker Chomerics Tecknit Consil®-II 842 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Tensile Strength | 0.827 MPa | 120 psi | Die A; ASTM D412 |
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 0.827 MPa | >= 120 psi | ASTM D412 |
Monmouth Rubber & Plastics Durafoamâ„¢ S88 PVC/NBR Information provided by Monmouth Rubber & Plastics Corp. |