Material Notes:
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, is designed for applications requiring low compression forces.Molded onlyRoHS CompliantInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.45 g/cc
1.32 - 1.45 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 33 - 47
33 - 47
ASTM D2240
Tensile Strength >= 0.827 MPa
>= 120 psi
ASTM D412
Elongation at Break >= 75 %
>= 75 %
ASTM D412
Compression Set <= 25 %

@Temperature 100 °C,
Time 252000 sec
<= 25 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Method B
Thermal Properties Metric English Comments
Thermal Conductivity 0.600 W/m-K

@Pressure 2.07 MPa
4.16 BTU-in/hr-ft²-°F

@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flex TR10
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Volume Resistivity <= 0.25 ohm-cm
<= 0.25 ohm-cm
without pressure-sensitive adhesive; CEPS-0002
Shielding Effectiveness >= 0.60 dB

@Frequency 4.00e+10 Hz
>= 0.60 dB

@Frequency 4.00e+10 Hz
Plane Wave; Method 1, CHO-TM-TP08
>= 70 dB

@Frequency 2.00e+9 Hz
>= 70 dB

@Frequency 2.00e+9 Hz
Plane Wave; Method 1, CHO-TM-TP08
>= 70 dB

@Frequency 1.00e+10 Hz
>= 70 dB

@Frequency 1.00e+10 Hz
Plane Wave; Method 1, CHO-TM-TP08
>= 75 dB

@Frequency 1.00e+8 Hz
>= 75 dB

@Frequency 1.00e+8 Hz
E-Field; Method 1, CHO-TM-TP08
>= 75 dB

@Frequency 5.00e+8 Hz
>= 75 dB

@Frequency 5.00e+8 Hz
E-Field; Method 1, CHO-TM-TP08
Descriptive Properties Value Comments
Binder Silicone
Filler Ni/C
Heat Aging <0.25 ohm-cm
150°C for 48 hr, CEPS-0002