Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 13.46 MPa @Treatment Temp. 121 °C, Time 605000 sec |
1952 psi @Treatment Temp. 250 °F, Time 168 hour |
Air Oven aged; UL1581 |
S&E Specialty Polymers CPE-01-266A-405 Black PVC Application: 90° C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced tear properties and flexibility.Information provided by S&E Specialty Polymers |