Polymer Property : Tensile Strength = 1952 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 13.46 MPa

@Treatment Temp. 121 °C,
Time 605000 sec
1952 psi

@Treatment Temp. 250 °F,
Time 168 hour
Air Oven aged; UL1581
S&E Specialty Polymers CPE-01-266A-405 Black PVC
Application: 90° C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced tear properties and flexibility.Information provided by S&E Specialty Polymers