Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Quantum PPS Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 89.6 MPa | 13000 psi | CW; ASTM D638 |
Haysite H1000 Polyester Laminate Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide.. |
|||
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Teknor Apex Beetle® 102 Nylon 66, Unreinforced, Nucleated Notes: Nucleated for fast cycling; Improved strength and rigidity; FMVSS Flammability: Passes, FMVSS 302Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Ensinger Tecapeek® XP-91 Compression Molded PEEK Compound, 30% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 89.6 MPa @Temperature 23.0 °C |
13000 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Tensile Strength | 89.6 MPa @Temperature 23.0 °C |
13000 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |
|||
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |
|||
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Quadrant EPP Quadrant Nylon 105 Black |
|||
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF10 FR BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackProcessing Method: Injection MoldingInformation provided by.. |
|||
Tensile Strength | 89.6 MPa | 13000 psi | ASTM D638 |
Techmer ES HiFill FR® PBT GF15 FR X 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, In.. |