Polymer Property : Tensile Strength = 138 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 138 MPa
20000 psi
ASTM D638
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet)
Tensile Strength 138 MPa
20000 psi
ASTM D638
Quantum PEEK 30% Carbon Filled
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 138 MPa
20000 psi
ASTM D638
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC
LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance..
Tensile Strength 138 MPa
20000 psi
ASTM D638
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet)
Tensile Strength 138 MPa
20000 psi
ASTM D638
Techmer ES Luriblend® PA6/6 GF30 ML5 HS BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and He..
Tensile Strength >= 138 MPa
>= 20000 psi
Machine or Cross; IPC TM-650 2.4.18.3
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs
For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance..
Tensile Strength >= 138 MPa
>= 20000 psi
IPC TM-650 2.4.18
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs
For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d..
Tensile Strength 138 MPa
20000 psi
Anderman Ceramics EA95 Sintered Alumina, 95%
Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. ..
Tensile Strength >= 138 MPa
>= 20000 psi
IPC TM-650 2.4.18
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite
Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a..
Tensile Strength 138 MPa
20000 psi
ASTM D638
Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled
Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistanc..
Tensile Strength 138 MPa

@Temperature 23.0 °C
20000 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
Tensile Strength 138 MPa

@Temperature 23.0 °C
20000 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers