Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 138 MPa | 20000 psi | ASTM D638 |
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet) |
|||
Tensile Strength | 138 MPa | 20000 psi | ASTM D638 |
Quantum PEEK 30% Carbon Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 138 MPa | 20000 psi | ASTM D638 |
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
Tensile Strength | 138 MPa | 20000 psi | ASTM D638 |
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet) |
|||
Tensile Strength | 138 MPa | 20000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 GF30 ML5 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and He.. |
|||
Tensile Strength | >= 138 MPa | >= 20000 psi | Machine or Cross; IPC TM-650 2.4.18.3 |
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance.. |
|||
Tensile Strength | >= 138 MPa | >= 20000 psi | IPC TM-650 2.4.18 |
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d.. |
|||
Tensile Strength | 138 MPa | 20000 psi | |
Anderman Ceramics EA95 Sintered Alumina, 95% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Tensile Strength | >= 138 MPa | >= 20000 psi | IPC TM-650 2.4.18 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Tensile Strength | 138 MPa | 20000 psi | ASTM D638 |
Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistanc.. |
|||
Tensile Strength | 138 MPa @Temperature 23.0 °C |
20000 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
Tensile Strength | 138 MPa @Temperature 23.0 °C |
20000 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |