Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 2.07 MPa | >= 300 psi | ASTM D412 |
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer Description: CONSIL-RHT 855 is a pure silver-filled silicone elastomer ideal for applications where high temperature is a concernTypical Applications: CONSIL-RHT 855 silicone is used throughout indu.. |
|||
Tensile Strength | 2.07 MPa @Strain 100 % |
300 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 2.07 MPa @Strain 100 % |
300 psi @Strain 100 % |
Type IV, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tensile Strength | 2.07 MPa @Strain 100 % |
300 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 2.07 MPa | 300 psi | Measured on solution cast film from toluene; BAM 1245 |
Kraton® G1642 H (SEBS) Linear Triblock Copolymer Description: Kraton G1642 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | 2.07 MPa | 300 psi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® G1701 H (SEP) Linear Diblock Copolymer Description: Kraton G1701 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | 2.07 MPa | 300 psi | Side 2, Silicone Property; ASTM D412 |
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value.. |
|||
Tensile Strength | 2.07 MPa | 300 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S.. |
|||
Tensile Strength | 2.07 MPa | 300 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val.. |
|||
Tensile Strength | >= 2.07 MPa | >= 300 psi | Compound Property |
Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported Design/Construction:Overall: Fully cured/unsupported This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.In.. |
|||
Tensile Strength | 2.07 MPa | 300 psi | ASTM D412 |
Kraton® G1701 M (SEP) Linear Diblock Copolymer Description: Kraton G1701 M is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | 2.07 MPa | 300 psi | Typical properties of film cast from toluene solution; ASTM D412 |