Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 290 MPa | 42100 psi | ASTM D-638 |
PlastiComp Velocity® LCF40-PA6 High Flow Nylon 6, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Tensile Strength | 290 MPa | 42100 psi | ASTM D-638 |
PlastiComp Complet® LCF40 - PA6 Nylon 6, 40% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Tensile Strength | 290 MPa | 42100 psi | |
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crysta.. |
|||
Tensile Strength | 290 MPa | 42000 psi | |
Anderman Ceramics EAZ 20 Zirconia Toughened Alumina Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |