Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D412 |
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D412 |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D412 |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax CCP PBT 1100-211X Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1100-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1100-211S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | >= 49.0 MPa | >= 7110 psi | ASTM D 638 |
Karina 80/201-D-SD Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | |
Henkel Hysol EA 9321 Paste Adhesive System Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1100-211XG Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | |
Taiwan Sheen Soon Sheenthane® A8900F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | |
Taiwan Sheen Soon Sheenthane® A9315E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | |
Taiwan Sheen Soon Sheenthane® A9519UK Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 49.0 MPa | 7100 psi | ASTM D638 |
Techmer ES HiFill® ABS HI 0300 High Impact Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Density and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by .. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® T102 PET, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D638 |
Samyang Trimma® SD6320P PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | |
Taiwan Sheen Soon Sheenthane® A9610 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D412 |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D412/D638 |
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo.. |
|||
Tensile Strength | 49.0 - 62.7 MPa | 7100 - 9100 psi | |
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1100-211MB Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Tensile Strength | 49.0 - 58.8 MPa | 7110 - 8530 psi | ASTM D638 |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Tensile Strength | 49.0 MPa | 7110 psi | ASTM D638 |
Samyang Trimma® SD6350T PMMA, Opaque High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |