Mechanical Properties Metric English Comments
Tensile Strength 4.48 MPa
650 psi
ASTM D412
S&E Specialty Polymers GTPR-1358A
Thermoplastic Rubber material designed for winter boot applications requiring excellent abrasion and stitch tear.  Available in a wide range of colors.Information provided by S&E Specialty Polymer..
Tensile Strength >= 4.48 MPa
>= 650 psi
ASTM D412
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Tensile Strength >= 4.48 MPa
>= 650 psi
ASTM D412
Parker Chomerics Tecknit SC-Consil® FR862 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Tensile Strength 4.48 MPa

@Strain 100 %
650 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 4.48 MPa
650 psi
Teknor Apex Tekbond® TB 2007 Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
Tensile Strength 4.48 MPa
650 psi
ASTM D412
Teknor Apex Telcar® OBC 4945A Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Tensile Strength 4.48 MPa
650 psi
ASTM D412
Teknor Apex Telcar® OBC 4945F Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Tensile Strength 4.48 MPa
650 psi
Silicone Property; ASTM D412
Arlon 49442R0075 0.0075" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassThis data represents typical values for the production material and should not be used as material specifications.I..
Tensile Strength 4.48 MPa
650 psi
Compound Property; ASTM D412
Arlon 49442R0075EP 0.0075" (0.190 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Substrate: Style 1681 FiberglassSide 2: Acrylic PSAThis data Represents typical values for the production material. The data should not be used to w..
Tensile Strength 4.48 MPa
650 psi
Silicone Property; ASTM D412
Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Uncured Silicone Rubber Substrate: Style 7628 FiberglassSide 2: Cured Silicone RubberAppearan..
Tensile Strength 4.48 MPa
650 psi
Silicone Property; ASTM D412
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim..
Tensile Strength 4.48 MPa
650 psi
Silicone Property; ASTM D412
Arlon Thermabond® T20 (99710W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 15 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Pri..
Tensile Strength >= 4.48 MPa
>= 650 psi
Compound Property
Arlon CP-339R Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Tensile Strength >= 4.48 MPa
>= 650 psi
ASTM D412
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer
Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics
Tensile Strength >= 4.48 MPa
>= 650 psi
ASTM D412
Parker Chomerics Tecknit SC-Consil® 861 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..