Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Silicone; Arlon SQA-TMS-003
140 microns
5.50 mil
Substrate; Arlon SQA-TMS-003
191 microns
7.50 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property; ASTM D2240
Tensile Strength 4.48 MPa
650 psi
Silicone Property; ASTM D412
Elongation at Break 250 %
250 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test 3.0
3.0
Inches; Char Length; Arlon SQA-TMS-019
25
25
Seconds; Flame and Glow Time; Arlon SQA-TMS-019
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 12
Arlon SQA-TMS-025
Uncoated Fabric Break Strength (lb/in) 110
Fill Direction, Substrate Property
195
Warp Direction, Substrate Property