Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 106 MPa | 15400 psi | |
Ohio Carbon Blank OCB AR-12 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Compressive Strength | 106 MPa | 15400 psi | ASTM D790 |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Compressive Strength | 106 MPa | 15400 psi | |
BCC Products BC 7053 Epoxy Casting BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding.. |