Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 114 MPa | 16500 psi | |
Ohio Carbon Blank OCB AR-08 EDM Grade Graphite Available in a range of sizes and shapes. |
|||
Compressive Strength | 114 MPa | 16500 psi | Ultimate; TM R050-38 |
Resinlab® EP965LVLX Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Compressive Strength | 114 MPa | 16500 psi | Break; TM R050-38 |
Resinlab® EP965LVLX Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Compressive Strength | 114 MPa | 16500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 114 - 141 MPa | 16500 - 20500 psi | |
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Break; TM R050-38 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Break; TM R050-38 |
Resinlab® EP965LVLX Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Compressive Strength | 114 MPa | 16500 psi | Ultimate; TM R050-38 |
Resinlab® EP965LVLX Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Compressive Strength | 114 MPa | 16500 psi | Break; TM R050-38 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Ultimate; TM R050-38 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Compressive Strength | 114 MPa | 16500 psi | Ultimate; TM R050-38 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |