Polymer Property : Compressive Strength = 15.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 15.2 MPa
2200 psi
ASTM D695
ScanTube FEP Tubing
Information provided by ScanTube, Inc.
Compressive Strength 15.2 MPa
2200 psi
ASTM D695
ScanTube MFA Tubing
Information provided by ScanTube, Inc.
Compressive Strength 15.2 MPa
2200 psi
ASTM D695
ScanTube PFA Tubing
Information provided by ScanTube, Inc.
Compressive Strength 15.2 MPa
2200 psi
ASTM D-695
CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board
REN Shape 460 is a moderate density precision modeling board that features a lower coefficient of thermal expansion to provide enhanced dimensional stability over a broader temperature range than ot..
Compressive Strength 15.2 MPa
2200 psi
ultimate load
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact
These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou..
Compressive Strength 15.2 MPa
2200 psi
BCC Products MB 1300 Polyurethane Foam Modeling Board
MB 1300 is a Mahogany colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1300 is medium low density foam of approximately 30lbs/ft3 board. Easily cut using CNC machining equi..