Material Notes:
Information provided by ScanTube, Inc.
Physical Properties Metric English Comments
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
Water Absorption <= 0.030 %
<= 0.030 %
ASTM D257
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM D2240
Tensile Strength 24.1 MPa
3500 psi
ASTM D638, ASTM D1708
Elongation at Break 300 %
300 %
ASTM D638, ASTM D1708
Tensile Modulus 0.276 GPa
40.0 ksi
ASTM D638
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
Compressive Strength 15.2 MPa
2200 psi
ASTM D695
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.202 W/m-K
1.40 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 285 °C
545 °F
Maximum Service Temperature, Air 240 °C
464 °F
Continuous
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C
149 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.1

@Frequency 1000 Hz
2.1

@Frequency 1000 Hz
ASTM D150
2.1

@Frequency 1.00e+6 Hz
2.1

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 78.7 kV/mm
2000 kV/in
Short Term; 10 mil film; ASTM D149
Dissipation Factor 0.00020

@Frequency 1000 Hz
0.00020

@Frequency 1000 Hz
ASTM D150
0.00030

@Frequency 1.00e+6 Hz
0.00030

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Chemical Resistance Excellent
Weather Resistance Excellent
Users viewing this material also viewed the following: