Mechanical Properties Metric English Comments
Compressive Strength 155 MPa
22500 psi
Poco Graphite Glassmate® LT Graphite
In very high wear situations, LT, with a hardness rating higher than GM material, will resist wear longer.
Compressive Strength 155 MPa
22500 psi
ASTM D695
IDI Composites 44-10 HGM Thermoset Polyester, Molding
Same as 44-10 HG with Mil Spec MAI-60.Data provided by the manufacturer.
Compressive Strength 155 MPa
22500 psi
SGL Carbon Group EK 20 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 155 MPa
22500 psi
ASTM D695
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
Compressive Strength 155 MPa
22500 psi
ASTM D695
Plenco 1510 Polyester, Pellet, Injection Molded
PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file ..
Compressive Strength 155 MPa
22500 psi
ASTM D695
Plenco 3554 Phenolic, Granular, Compression Molded
PLENCO 03554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 03554 is available in black. It is UL listed. 03554 is a re-numbe..
Compressive Strength 155 MPa
22500 psi
Absolute Drying; ASTM-D695
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Compressive Strength 155 MPa
22500 psi
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.