Poco Graphite Glassmate® LT Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name Glassmate®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite Glassmate® LT Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
In very high wear situations, LT, with a hardness rating higher than GM material, will resist wear longer.
Physical Properties Metric English Comments
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Particle Size 5.0 µm
5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 96
96
Flexural Strength 86.0 MPa
12500 psi
Compressive Strength 155 MPa
22500 psi
Thermal Properties Metric English Comments
CTE, linear 8.50 µm/m-°C
4.72 µin/in-°F
Thermal Conductivity 60.0 W/m-K
416 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00245 ohm-cm
0.00245 ohm-cm
Descriptive Properties Value Comments
Oxidation Threshold 470°C