Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 128 MPa | 18500 psi | Ultimate; TM R050-38 |
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11.. |
|||
Compressive Strength | 128 MPa | 18500 psi | Ultimate; TM R050-38 |
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11.. |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-309N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-309NM,Body Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-309T Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-322T Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 127 MPa | <= 18500 psi | Cold Crushing Strength |
Chosun Refractories CSN-332N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |