Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.10 - 3.20 g/cc
0.112 - 0.116 lb/in³
Porosity 2.0 - 5.0 %
2.0 - 5.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Compressive Strength <= 127 MPa
<= 18500 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 71 - 76 %
71 - 76 %
Carbon, C 8.0 - 11 %
8.0 - 11 %
ZrO2 6.0 - 8.0 %
6.0 - 8.0 %
Descriptive Properties Value Comments
Remarks Tar impregnated, Spalling resistance, Corrosion resistance