Polymer Property : Compressive Strength = 234 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 234 MPa
33900 psi
ASTM D695
Resinoid 1363 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Compressive Strength 234 MPa
33900 psi
ASTM D695
IDI Composites 46-16-60 Thermoset Polyester, Sheet
TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer.
Compressive Strength 234 MPa
33900 psi
ASTM D695
IDI Composites C-210 Thermoset Polyester, Sheet
CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by ..
Compressive Strength 234 MPa
33900 psi
ASTM D695
IDI Composites E-207 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Compressive Strength 234 MPa

@Thickness 12.7 mm
34000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP310 Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500".
Compressive Strength 234 MPa

@Thickness 12.7 mm
34000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP310E Cotton Fabric
Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M..
Compressive Strength 234 MPa

@Thickness 12.7 mm
34000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP329 Cotton Fabric
Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, ..
Compressive Strength 234 MPa
33900 psi
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..
Compressive Strength 234 MPa
33900 psi
Haysite H258 Polyester Laminate
Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications..
Compressive Strength 234 MPa
33900 psi
Haysite H260 Polyester Laminate
Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m..
Compressive Strength 234 MPa
33900 psi
ASTM D695
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic
RXÂ 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro..
Compressive Strength 234 - 241 MPa
34000 - 35000 psi
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..
Compressive Strength 234 MPa

@Thickness 12.7 mm
34000 psi

@Thickness 0.500 in
ASTM D695
Industrial Laminates/Norplex NP321 Cotton Fabric  (discontinued **)
Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f..