Material Notes:
Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet material, it may be used as dedicated or adjustable flow solder carriers as well as surface mount pallets. Standard color is blue/grey. Available thicknesses from 1/8" to 1/2" and 4mm to 12mm. Sheet sizes are 36" X 72" and 48" X 60", special thicknesses and custom sheet sizes are available.
Physical Properties Metric English Comments
Density 1.98 g/cc
0.0715 lb/in³
ASTM D572
Water Absorption 0.16 %
0.16 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 52
52
Tensile Strength, Ultimate 110 MPa
16000 psi
Flexural Strength 172 MPa
24900 psi
Flexural Modulus 12.0 GPa
1740 ksi
Compressive Strength 234 MPa
33900 psi
Shear Strength 103 MPa
14900 psi
ASTM D732
Izod Impact, Notched 5.40 J/cm
10.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 300 °C
>= 572 °F
Service Operating temperature.
Electrical Properties Metric English Comments
Surface Resistance 1e+05 - 1.00e+9 ohm
1e+05 - 1.00e+9 ohm
Ohm; ASTM D257