Polymer Property : Compressive Strength = 33900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 234 MPa
33900 psi
ASTM D695
Resinoid 1363 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Compressive Strength 234 MPa
33900 psi
ASTM D695
IDI Composites 46-16-60 Thermoset Polyester, Sheet
TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer.
Compressive Strength 234 MPa
33900 psi
ASTM D695
IDI Composites C-210 Thermoset Polyester, Sheet
CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by ..
Compressive Strength 234 MPa
33900 psi
ASTM D695
IDI Composites E-207 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Compressive Strength 234 MPa
33900 psi
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..
Compressive Strength 234 MPa
33900 psi
Haysite H258 Polyester Laminate
Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications..
Compressive Strength 234 MPa
33900 psi
Haysite H260 Polyester Laminate
Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m..
Compressive Strength 234 MPa
33900 psi
ASTM D695
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic
RXÂ 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro..