Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 282 MPa | 40900 psi | SABIC Method |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Compressive Strength | 282 MPa | 40900 psi | ASTM D695 |
Plenco 6401 Phenolic, Briquette, Transfer Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |