Polymer Property : Compressive Strength = 40900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 282 MPa
40900 psi
SABIC Method
SABIC Innovative Plastics LNP VERTON EV008 PEI
LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural.
Compressive Strength 282 MPa
40900 psi
ASTM D695
Plenco 6401 Phenolic, Briquette, Transfer Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.