SABIC Innovative Plastics LNP VERTON EV008 PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON EV008 PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm

@Time 86400 sec
0.0030 - 0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 187 MPa
27100 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.5 %
1.5 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 15.1 GPa
2190 ksi
5 mm/min; ASTM D638
Flexural Strength 268 MPa
38900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 14.4 GPa
2090 ksi
1.3 mm/min, 50 mm span; ASTM D790
Compressive Strength 282 MPa
40900 psi
SABIC Method
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
Izod Impact, Unnotched 0.420 J/cm
0.787 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
8.33 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 41.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 206 °C

@Thickness 3.20 mm
403 °F

@Thickness 0.126 in
unannealed; ASTM D648