Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 290 MPa | 42000 psi | |
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |
|||
Compressive Strength | 290 MPa | 42100 psi | Flatwise; ASTM D695 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |
|||
Compressive Strength | 290 MPa @Thickness 12.7 mm |
42000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP193M Synthetic Fabric Base Grade Description: 17 oz. aramide and “soft glass†fibers are combined to make a fabric that is stronger than pure aramide and less abrasive than glass fabrics. This material is impregnated with.. |
|||
Compressive Strength | 290 MPa | 42000 psi | ASTM D695 |
Haysite H320 Polyester Composite A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ.. |
|||
Compressive Strength | 290 MPa | 42000 psi | |
SGL Carbon Group EK 305 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |