Polymer Property : Compressive Strength = 42100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 290 MPa
42100 psi
Flatwise; ASTM D695
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3)
Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product.