Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Glastic
Trade Name Laminates/Shapes
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 50
50
ASTM D2583
Tensile Strength, Ultimate 103 MPa
14900 psi
ASTM D638
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Flexural Strength 172 MPa
24900 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Compressive Strength 140 MPa
20300 psi
Edgewise; ASTM D695
290 MPa
42100 psi
Flatwise; ASTM D695
Shear Strength 100 MPa
14500 psi
ASTM D732
Izod Impact, Notched 5.10 J/cm
9.55 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.270 W/m-K
1.87 BTU-in/hr-ft²-°F
ASTM C177
UL RTI, Electrical 130 °C
266 °F
UL 746B
UL RTI, Mechanical with Impact 160 °C
320 °F
UL 746B
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 8.00 kV/mm
203 kV/in
Perpendicular, Short-term, in air; ASTM D149
Arc Resistance 185 sec
185 sec
ASTM D495