Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 212 MPa | 30700 psi | ASTM D695 |
Plenco 2000 Phenolic, Granular, Compression Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Compressive Strength | 212 MPa | 30700 psi | ASTM D695 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Compressive Strength | 212 MPa | 30700 psi | ASTM D695 |
Plenco 2571 Phenolic, Granular, Compression Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Compressive Strength | 212 MPa | 30700 psi | ASTM D695 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Compressive Strength | 212 MPa | 30700 psi | ASTM D695 |
Plenco 2300 Phenolic, Granular, Transfer Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Compressive Strength | 212 MPa | 30700 psi | ASTM D695 |
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Compressive Strength | 212 MPa | 30700 psi | ASTM D695 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |