Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 2308 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2308 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is available in black or brown color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.39 %
0.39 %
ASTM D570
Linear Mold Shrinkage 0.0048 cm/cm
0.0048 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 89
89
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 0.66 %
0.66 %
ASTM D638
Tensile Modulus 8.50 GPa
1230 ksi
ASTM D638
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 8.20 GPa
1190 ksi
ASTM D790
Compressive Strength 212 MPa
30700 psi
ASTM D695
Izod Impact, Notched 0.194 J/cm
0.363 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.192 J/cm²
0.914 ft-lb/in²
ASTM D256
Impact 115
115
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 74.0 µm/m-°C

@Temperature 40.0 - 130 °C
41.1 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.410 W/m-K

@Temperature 100 °C
2.85 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 200 °C
392 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 176 °C
349 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.248 %
0.248 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 9.80e+11 ohm-cm
9.80e+11 ohm-cm
ASTM D247
Dielectric Constant 4.8
4.8
ASTM D150
Dielectric Strength 14.2 kV/mm
361 kV/in
Short Time; ASTM D149
Dissipation Factor 0.041
0.041
ASTM D150
Arc Resistance 122 sec
122 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638