Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 43.0 MPa | 6240 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 43.0 MPa | 6240 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Dry Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 43.0 MPa @Time 3.60e+7 sec |
6240 psi @Time 10000 hour |
|
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Compressive Strength | 43.0 MPa @Time 360000 sec |
6240 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed.. |