Polymer Property : Compressive Strength = 6240 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 43.0 MPa
6240 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned
Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 43.0 MPa
6240 psi
10% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Dry
Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 43.0 MPa

@Time 3.60e+7 sec
6240 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
Compressive Strength 43.0 MPa

@Time 360000 sec
6240 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy
Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed..