Mechanical Properties Metric English Comments
Compressive Strength 550 MPa
79800 psi
ICE Steatite L-4
Data provided by the manufacturer, International Ceramic Engineering.
Compressive Strength 550 MPa
79800 psi
ASTM C773
CoorsTek Mullite, S2
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Compressive Strength 550 MPa

@Thickness >=5.00 mm
79800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Compressive Strength 550 MPa

@Thickness >=5.00 mm
79800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t..
Compressive Strength 550 MPa

@Thickness >=5.00 mm
79800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Compressive Strength 550 MPa

@Thickness >=5.00 mm
79800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Compressive Strength 550 MPa

@Thickness >=5.00 mm
79800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..