Mechanical Properties Metric English Comments
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented, 2.2 m/s, ductile; ASTM D3763
Phillips Sumika Marlex® CBF-300 Talc-Filled High Flow Thermoplastic Olefin  (discontinued **)
Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued ..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Prevex VFAX PPE+PS
High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region.
Impact Test 17.0 J

@Temperature -30.0 °C
12.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced
PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro..
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced
PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro..
Impact Test 17.0 J

@Thickness 4.00 mm
12.5 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Impact Test 17.0 J

@Thickness 102 mm
12.5 ft-lb

@Thickness 4.00 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)
AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu..
Impact Test 17.0 J

@Thickness 4.00 mm
12.5 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R451-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..
Impact Test 17.0 J

@Thickness 1.70 mm
12.5 ft-lb

@Thickness 0.0669 in
ASTM D2794-93
3M Scotchkote™ 2400 Pipe Renewal Liner
3M Scotchkote Pipe Renewal Liner 2400 has been specifically developed for the rehabilitation of potable water pipe infrastructure to help extend service life, reduce leaks, and improve water quality..
Impact Test 17.0 J

@Thickness 4.00 mm
12.5 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix