Polymer Property : 100% Modulus = 0.00210 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00210 GPa
0.305 ksi
ISO/R527
Polykemi AB POLYelast TPE ZS2606 Thermoplastic Elastomer, SEBS/SBS-based
Information provided by Polykemi AB
100% Modulus 0.00210 GPa
0.305 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00210 GPa
0.304 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00210 GPa
0.305 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
100% Modulus 0.00210 GPa
0.305 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s..
100% Modulus 0.00210 GPa
0.304 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N990 (MT) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00210 GPa
0.305 ksi
ASTM D412
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
100% Modulus 0.00210 GPa
0.305 ksi
ASTM D412
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
100% Modulus 0.00210 GPa
0.305 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR Di-Cup 40C
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00210 GPa
0.305 ksi
ASTM D412
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
100% Modulus 0.00210 GPa
0.305 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00210 - 0.00600 GPa
0.305 - 0.870 ksi
ASTM D 638
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
100% Modulus 0.00210 GPa
0.305 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR Di-Cup 40C
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00210 GPa
0.305 ksi
ISO 37
AlphaGary Evoprene™ G 958 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..