Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00210 GPa | 0.305 ksi | ISO/R527 |
Polykemi AB POLYelast TPE ZS2606 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | ASTM D412 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | ASTM D412 |
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | ASTM D412 |
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00210 - 0.00600 GPa | 0.305 - 0.870 ksi | ASTM D 638 |
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR Di-Cup 40C MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00210 GPa | 0.305 ksi | ISO 37 |
AlphaGary Evoprene™ G 958 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |