Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
ASTM D412
Tensile Strength at Break 18.9 MPa
2740 psi
ASTM D412
Elongation at Break 540 %
540 %
ASTM D412
100% Modulus 0.00210 GPa
0.305 ksi
ASTM D412
200% Modulus 0.00540 GPa
0.783 ksi
ASTM D412
300% Modulus 0.00980 GPa
1.42 ksi
ASTM D412
Tear Strength 45.0 kN/m
257 pli
ASTM D2240