Mechanical Properties Metric English Comments
100% Modulus 0.00280 GPa
0.406 ksi
ISO/R527
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based
Information provided by Polykemi AB
100% Modulus 0.00280 GPa
0.406 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D638
Multibase Multi-Flex® TPE A 5801 LC BLK
Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and fe..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
100% Modulus 0.00280 GPa
0.406 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8068B Thermoplastic Elastomer
Elastocon® 8068B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068B is well suited for consumer goods an..
100% Modulus 0.00280 GPa
0.406 ksi
Dow AFFINITY™ EG 8150 Polyolefin Elastomer
AFFINITY® EG 8150 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation It ex..
100% Modulus 0.00280 GPa
0.406 ksi
Dow AFFINITY™ EG 8200 Polyolefin Elastomer
AFFINITY® EG 8200 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation. It e..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412
Advanced Polymer Alloys Alcryn® 2170 NC Melt Processable Rubber
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412
Advanced Polymer Alloys DuraGrip™ DGR 6170 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6170 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6, Nylon 6/6, glass filled Nylo..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane
Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412; ASTM D638
Lubrizol Estane® 58252 Thermoplastic Polyurethane
Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon..
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412-80
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Gum Compound  (discontinued **)&
Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Physical property data below (..
100% Modulus 0.00280 GPa
0.406 ksi
ISO 37
AlphaGary Evoprene™ GC 5683 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
100% Modulus 0.00280 GPa
0.406 ksi
ISO 37
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins