Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78

@Time 5.00 sec
72 - 78

@Time 0.00139 hour
ASTM D2240
Tensile Strength 37.9 MPa
5500 psi
ASTM D412
Elongation at Break 680 %
680 %
ASTM D412
100% Modulus 0.00280 GPa
0.406 ksi
ASTM D412
300% Modulus 0.00410 GPa
0.595 ksi
ASTM D412
Tear Strength 17.5 kN/m
100 pli
ASTM D470
Graves Tear Strength 52.6 kN/m
300 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 6.4
6.4
H18, 1000g; ASTM D3389 B
Tensile Set 6.0 %
6.0 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
Kofler
110 °C
230 °F
DSC
Glass Transition Temp, Tg -30.0 °C
-22.0 °F
DSC
Processing Properties Metric English Comments
Zone 1 166 °C
331 °F
Extrusion
Zone 2 171 °C
340 °F
Extrusion
Zone 3 176 °C
349 °F
Extrusion
Zone 4 182 °C
360 °F
Extrusion
Adapter Temperature 182 °C
360 °F
Extrusion
Die Temperature 182 °C
360 °F
Zone 1, Extrusion
182 °C
360 °F
Zone 2, Extrusion
Drying Temperature 54.0 °C
129 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F