Polymer Property : 100% Modulus = 0.00350 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00350 GPa
0.508 ksi
DIN 53504
Huntsman IROGRAN® A 85 P 4854 Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 85 P 4854 is a flame-retardant, halogen-free polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4854 is part..
100% Modulus 0.00350 GPa
0.508 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N550 (FEF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00350 GPa
0.508 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 5565 General Purpose Molding
FormulationNordel® IP 5565
100% Modulus 0.00350 GPa
0.508 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
100% Modulus 0.00350 GPa
0.508 ksi
ISO 37
AlphaGary Evoprene™ GC 5651 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
100% Modulus 0.00350 GPa
0.508 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N550 (FEF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00350 GPa
0.508 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR7015 Plasticized Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
100% Modulus 0.00350 GPa
0.508 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1570 Polyester Based TPU
Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.