Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1570 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1570 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
ASTM D2240
Tensile Strength 30.0 MPa
4350 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
100% Modulus 0.00350 GPa
0.508 ksi
ASTM D412
300% Modulus 0.00650 GPa
0.943 ksi
ASTM D412
Tear Strength 75.0 kN/m
428 pli
ASTM D624
Abrasion 50
50
Abrasion resistance, mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 180 - 195 °C
356 - 383 °F
Users viewing this material also viewed the following: