Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00350 GPa | 0.508 ksi | DIN 53504 |
Huntsman IROGRAN® A 85 P 4854 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 85 P 4854 is a flame-retardant, halogen-free polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4854 is part.. |
|||
100% Modulus | 0.00350 GPa | 0.508 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N550 (FEF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00350 GPa | 0.508 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 General Purpose Molding FormulationNordel® IP 5565 |
|||
100% Modulus | 0.00350 GPa | 0.508 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00350 GPa | 0.508 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5651 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00350 GPa | 0.508 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N550 (FEF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00350 GPa | 0.508 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR7015 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00350 GPa | 0.508 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1570 Polyester Based TPU Plasticizer free, excellent abrasion & slip resistance, low temperature flexibility, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |